Highly Saturated Nitrile overcoated E glass cord (Elastomer Polymer Matrix Composite)
Adhesion
Fad55 N at 20 °C
min., T Test
Linear density
ρlinear1.25E-3 - 1.55E-3 g/cm at 20 °C
Loss on Ignition
LOI18 - 26 % at 20 °C
Bobbin Inner Diameter
db,i57 - 63 mm
tapered
Bobbin Length
lb341 mm
Diameter
d0.25 - 0.45 mm
Apparent Diameter
Flange Diameter
Df279.5 mm
Color
Black Overcoat
Cord Construction
110.1/0
Other
Manufacturing Location: UK
Processing history
Latex Type: HNBR
Twist per Meter
TPM130 - 154 TPM
Direction: S & Z
This material data has been provided by NGF Glass.