Highly Saturated Nitrile overcoated E glass cord (Elastomer Polymer Matrix Composite)

This material data has been provided by NGF Glass.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Adhesion

23.0 °C

115 N

Show Supplier Material materials with Adhesion of 115 N

min., T Test

Linear density

23.0 °C

2.65E-3 - 3.11E-3 g/cm

Show Supplier Material materials with Linear density of 2.65E-3 - 3.11E-3 g/cm

Loss on Ignition

23.0 °C

20 - 24 %

Show Supplier Material materials with Loss on Ignition of 20 - 24 %

Dimension

PropertyValueComment

Bobbin Inner Diameter

57 - 63 mm

Show Supplier Material materials with Bobbin Inner Diameter of 57 - 63 mm

tapered

Bobbin Length

341 mm

Show Supplier Material materials with Bobbin Length of 341 mm

Diameter

0.4 - 0.54 mm

Show Supplier Material materials with Diameter of 0.4 - 0.54 mm

Apparent Diameter

Flange Diameter

279.5 mm

Show Supplier Material materials with Flange Diameter of 279.5 mm

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

1.6 - 2.8 %

Show Supplier Material materials with Elongation of 1.6 - 2.8 %

Nominal breaking force

23.0 °C

125 N

Show Supplier Material materials with Nominal breaking force of 125 N

Tensile Member: E Glass

Technological properties

Property
Color

Black Overcoat

Cord Construction

110.1/2

Other

Manufacturing Location: UK

Processing history

Latex Type: HNBR

Twist per Meter

130 - 154 TPM