Glass cord 979/980

Alternative and trade names
Glass Cord
Want to keep this datasheet? Save it now in your required format

Description

Highly Saturated Nitrile overcoated Carbon Fibre and E glass hybrid cord for Belt in Oil (Elastomer Polymer Matrix Composite)

This material data has been provided by NGF Glass.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Adhesion

23.0 °C

150 N

Show Supplier Material materials with Adhesion of 150 N

min., Peel

Linear density

23.0 °C

0.02 g/cm

Show Supplier Material materials with Linear density of 0.02 g/cm

Loss on Ignition

23.0 °C

19.5 - 27.5 %

Show Supplier Material materials with Loss on Ignition of 19.5 - 27.5 %

Dimension

PropertyValueComment

Bobbin Inner Diameter

57 - 63 mm

Show Supplier Material materials with Bobbin Inner Diameter of 57 - 63 mm

tapered

Bobbin Length

341 mm

Show Supplier Material materials with Bobbin Length of 341 mm

Diameter

1 - 1.3 mm

Show Supplier Material materials with Diameter of 1 - 1.3 mm

Apparent Diameter

Flange Diameter

279.5 mm

Show Supplier Material materials with Flange Diameter of 279.5 mm

Mechanical

PropertyTemperatureValueComment

Nominal breaking force

23.0 °C

1000 N

Show Supplier Material materials with Nominal breaking force of 1000 N

Tensile Member: Carbon Fibre & K Glass Hybrid

Technological properties

Property
Color

Black Overcoat

Cord Construction

400.1 - 22.3/12

Other

Manufacturing Location: UK

Processing history

Latex Type: HNBR

Twist per Meter

60 - 76 TPM

Direction: S & Z