Description

Epoxy / PU / TP Compatible U Glass High Tensile Yarn (Polymer Matrix Composite)

This material data has been provided by NGF Glass.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Linear density

23.0 °C

4.5E-4 - 6.8E-4 g/cm

Show Supplier Material materials with Linear density of 4.5E-4 - 6.8E-4 g/cm

Loss on Ignition

23.0 °C

0.3 - 0.6 %

Show Supplier Material materials with Loss on Ignition of 0.3 - 0.6 %

Mechanical

PropertyValue

Nominal breaking force

Tensile Member: U Glass

Technological properties

Property
Color

White

Cord Construction

Yarn

Other

Manufacturing Location: Japan

Processing history

Latex Type: Plastic Size

Twist per Meter

40 TPM