9 Micron High Tensile Roving

Alternative and trade names
Glass Roving
Want to keep this datasheet? Save it now in your required format

Description

Epoxy / PU / TP Compatible U Glass High Tensile Roving (Polymer Matrix Composite)

This material data has been provided by NGF Glass.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Linear density

23.0 °C

0 - 0.02 g/cm

Show Supplier Material materials with Linear density of 0 - 0.02 g/cm

Loss on Ignition

23.0 °C

0.3 - 0.6 %

Show Supplier Material materials with Loss on Ignition of 0.3 - 0.6 %

Dimension

PropertyValue

Bobbin Inner Diameter

76 mm

Show Supplier Material materials with Bobbin Inner Diameter of 76 mm

Mechanical

PropertyValue

Nominal breaking force

Tensile Member: U Glass

Technological properties

Property
Color

White

Cord Construction

Roving

Other

Manufacturing Location: Japan

Processing history

Latex Type: Plastic Size

Twist per Meter