CR Impregnated Chopped CF

Alternative and trade names
Glass Strand
Want to keep this datasheet? Save it now in your required format

Description

CR latex impregnated carbon fibre chopped strand (Elastomer Polymer Matrix Composite)

This material data has been provided by NGF Glass.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Linear density

23.0 °C

0.01 g/cm

Show Supplier Material materials with Linear density of 0.01 g/cm

Dimension

PropertyValue

Length

2 - 6 mm

Show Supplier Material materials with Length of 2 - 6 mm

Mechanical

PropertyValue

Nominal breaking force

Tensile Member: Carbon Fibre

Technological properties

Property
Color

Black

Other

Manufacturing Location: Canada

Processing history

Latex Type: CR, Dip Pick-Up: 9 to 13.5%