Description

A high-efficacy, extremely consistent glass flake glitter effects pigment from NSG

This material data has been provided by NGF Glass.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Flake thickness

1300 nm

Show Supplier Material materials with Flake thickness of 1300 nm

Linear density

23.0 °C

25 g/cm

Show Supplier Material materials with Linear density of 25 g/cm

Dimension

PropertyValueComment

Diameter

0.03 mm

Show Supplier Material materials with Diameter of 0.03 mm

Average

Technological properties

Property
Application areas

Strong, consistent glitter

Coating

Reduced Iron Oxide Coated

Color

Copper

Other

Glass Type: TA