Sub-Micron MEG025RY

Alternative and trade names
Glass Flake
Want to keep this datasheet? Save it now in your required format

Description

A high-efficacy, extremely consistent glass flake glitter effects pigment from NSG

This material data has been provided by NGF Glass.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Flake thickness

500 nm

Show Supplier Material materials with Flake thickness of 500 nm

Linear density

23.0 °C

25 g/cm

Show Supplier Material materials with Linear density of 25 g/cm

Dimension

PropertyValueComment

Diameter

0.03 mm

Show Supplier Material materials with Diameter of 0.03 mm

Average

Technological properties

Property
Application areas

Cosmetics, paints

Color

Yellow

Other

Glass Type: E