Sub-Micron MEG025TA

Alternative and trade names
Glass Flake
Want to keep this datasheet? Save it now in your required format

Description

A high-efficacy, extremely consistent glass flake glitter effects pigment from NSG

This material data has been provided by NGF Glass.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Flake thickness

500 nm

Show Supplier Material materials with Flake thickness of 500 nm

Linear density

23.0 °C

25 g/cm

Show Supplier Material materials with Linear density of 25 g/cm

Dimension

PropertyValueComment

Diameter

0.03 mm

Show Supplier Material materials with Diameter of 0.03 mm

Average

Technological properties

Property
Application areas

Cosmetics, paints

Color

Russett

Other

Glass Type: E