Microglas RCF-160T

Alternative and trade names
Glass Flake
Want to keep this datasheet? Save it now in your required format

Description

A glass flake based additive that provides wear resistance and tortuous fluid barrier

This material data has been provided by NGF Glass.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Flake thickness

5000 nm

Show Supplier Material materials with Flake thickness of 5000 nm

Linear density

23.0 °C

160 g/cm

Show Supplier Material materials with Linear density of 160 g/cm

Dimension

PropertyValueComment

Diameter

0.16 mm

Show Supplier Material materials with Diameter of 0.16 mm

Average

Technological properties

Property
Application areas

Protective Coatings

Color

Transparent

Other

Glass Type: C

Surface Treatment

Epoxy Silane