Epoxy RM130 - Rod

Alternative and trade names
NEMA GRADE: FR-4, U.L. LISTED: N
Want to keep this datasheet? Save it now in your required format

Description

Rolled and Molded Rods made from a glass fabric with a flame retardant resin system. RM130 combines excellent electrical characteristics with superior physical properties at normal operating temperatures. Electrical properties maintained in high humidity conditions. RM130 meets NEMA FR-4, but with elevated temperature performance.

This material data has been provided by Norplex Micarta.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.84 g/cm³

Show Supplier Material materials with Density of 1.84 g/cm³

ASTM D349

Moisture absorption

23.0 °C

0.1 %

Show Supplier Material materials with Moisture absorption of 0.1 %

ASTM D349, Condition D₁-24/23

Mechanical

PropertyTemperatureValueComment

Compressive strength

23.0 °C

363 MPa

Show Supplier Material materials with Compressive strength of 363 MPa

ASTM D349, Condition A

Flexural strength

23.0 °C

450 MPa

Show Supplier Material materials with Flexural strength of 450 MPa

ASTM D349, Condition A

Hardness, Rockwell M

23.0 °C

105 [-]

Show Supplier Material materials with Hardness, Rockwell M of 105 [-]

ASTM D349

Tensile strength

23.0 °C

284 MPa

Show Supplier Material materials with Tensile strength of 284 MPa

ASTM D349, Condition A

Thermal

PropertyValueComment

Relative temperature index, electrical

120 °C

Show Supplier Material materials with Relative temperature index, electrical of 120 °C

¹

Relative temperature index, mechanical strength

130 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C

¹

Flammability

UL 94, Class V-0

Technological properties

Property
Fillers

Glass Fabric

Other

1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use.

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".


To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest.


It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available.