General
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Compressive modulus | 23.0 °C | 7.58 MPa Show Supplier Material materials with Compressive modulus of 7.58 MPa | ASTM D695, Condition A |
Compressive strength | 23.0 °C | 251.7 - 293 MPa Show Supplier Material materials with Compressive strength of 251.7 - 293 MPa | ASTM D638, Condition E-1/150: T-150 (Min.) & A (Max.) |
Hardness, Rockwell M | 23.0 °C | 110 [-] Show Supplier Material materials with Hardness, Rockwell M of 110 [-] | ASTM D785 |
Tensile strength | 23.0 °C | 224.1 - 272.3 MPa Show Supplier Material materials with Tensile strength of 224.1 - 272.3 MPa | ASTM D638, Condition E-1/150: T-150 (Min.) & A (Max.) |
Thermal
Property | Value | Comment | |
---|---|---|---|
Glass transition temperature | 170 °C Show Supplier Material materials with Glass transition temperature of 170 °C | Min., DMA | |
Relative temperature index, electrical | 200 °C Show Supplier Material materials with Relative temperature index, electrical of 200 °C | ¹ | |
Relative temperature index, mechanical strength | 200 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 200 °C | ¹ | |
Flammability | UL Bulletin 94, Class HB |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Breakdown voltage | 23.0 °C | 60 - 65 kV Show Supplier Material materials with Breakdown voltage of 60 - 65 kV | ASTM D149, Condition A (Min.) & D-48/50 (Max.) |
Dielectric constant, 1MHz | 23.0 °C | 4.39 - 4.46 [-] Show Supplier Material materials with Dielectric constant, 1MHz of 4.39 - 4.46 [-] | ASTM D150, Condition A (Min.) & D-24/23 (Max.) |
Dielectric strength | 23.0 °C | 14.96 - 15.74 kV/mm Show Supplier Material materials with Dielectric strength of 14.96 - 15.74 kV/mm | ASTM D149, Condition D-48/50 (Min.) & A (Max.) |
Dissipation factor, 1MHz | 23.0 °C | 0.02 - 0.03 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 0.02 - 0.03 [-] | ASTM D150, Condition A (Min.) & D-24/23 (Max.) |
Technological properties
Property | ||
---|---|---|
Fillers | Glass Fabric | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use 2.The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |