Epoxy MC511FR - Sheet

Alternative and trade names
NEMA GRADE: FR-5, U.L. LISTED: N
Want to keep this datasheet? Save it now in your required format

Description

MC511FR is a high strength, medium weave glass epoxy laminate that retains a minimum of 50 percent of its room temperature flexural strength when tested at 150ᵒC. MC511FR also complies with MIL-I-24768/28, Type GEB-F.

This material data has been provided by Norplex Micarta.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bonding strength

23.0 °C

680 - 726 Kg

Show Supplier Material materials with Bonding strength of 680 - 726 Kg

ASTM D229, Condition A (Max.) & D-48/50 (Min.)

Density

23.0 °C

1.95 g/cm³

Show Supplier Material materials with Density of 1.95 g/cm³

ASTM D792

Moisture absorption

23.0 °C

0.05 %

Show Supplier Material materials with Moisture absorption of 0.05 %

ASTM D570, Condition D₁-24/23

Mechanical

PropertyTemperatureValueComment

Compressive strength

23.0 °C

482.63 MPa

Show Supplier Material materials with Compressive strength of 482.63 MPa

ASTM D695, Condition A, Flatwise

Flexural modulus

23.0 °C

22.75 GPa

Show Supplier Material materials with Flexural modulus of 22.75 GPa

ASTM D790, Condition A

Flexural modulus, transverse

23.0 °C

21.37 GPa

Show Supplier Material materials with Flexural modulus, transverse of 21.37 GPa

ASTM D790, Condition A

Flexural strength

23.0 °C

351.63 - 420.58 MPa

Show Supplier Material materials with Flexural strength of 351.63 - 420.58 MPa

ASTM D790, Condition E-1/150: T-150 (Min.) & A (Max.)

Flexural strength, transverse

23.0 °C

317.56 - 358.53 MPa

Show Supplier Material materials with Flexural strength, transverse of 317.56 - 358.53 MPa

ASTM D790, Condition E-1/150: T-150 (Min.) & A (Max.)

Hardness, Rockwell M

23.0 °C

115 [-]

Show Supplier Material materials with Hardness, Rockwell M of 115 [-]

ASTM D785

Impact strength, Izod notched, ASTM

23.0 °C

790 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 790 J/m

ASTM D256, Condition A

Impact strength, Izod notched, ASTM, Transversal

23.0 °C

598 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM, Transversal of 598 J/m

ASTM D256, Condition A

Shear strength, transverse

23.0 °C

268.89 MPa

Show Supplier Material materials with Shear strength, transverse of 268.89 MPa

ASTM D732

Tensile strength

23.0 °C

282.68 MPa

Show Supplier Material materials with Tensile strength of 282.68 MPa

ASTM D638, Condition A

Tensile strength, transverse

23.0 °C

220.63 MPa

Show Supplier Material materials with Tensile strength, transverse of 220.63 MPa

ASTM D638, Condition A

Thermal

PropertyValueComment

Glass transition temperature

190 °C

Show Supplier Material materials with Glass transition temperature of 190 °C

DMA

Relative temperature index, electrical

170 °C

Show Supplier Material materials with Relative temperature index, electrical of 170 °C

UL Bulletin 746b²

Relative temperature index, mechanical strength

180 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 180 °C

UL Bulletin 746b²

Flammability

UL 94, Class V-1

Electrical

PropertyTemperatureValueComment

Breakdown voltage

23.0 °C

60 - 70 kV

Show Supplier Material materials with Breakdown voltage of 60 - 70 kV

ASTM D149, Condition D-48/50 (Min.) & A (Max.)

Dielectric constant, 1MHz

23.0 °C

5.02 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 5.02 [-]

ASTM D150, Condition D₁24/23

Dielectric strength

23.0 °C

7.87 kV/mm

Show Supplier Material materials with Dielectric strength of 7.87 kV/mm

ASTM D149, Condition A

Dissipation factor, 1MHz

23.0 °C

0.02 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 0.02 [-]

ASTM D150, Condition D₁24/23

Technological properties

Property
Application areas

Typical applications include structural applications when used in elevated temperatures.

Fillers

Glass Fabric

Other

1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use


2.The mechanical properties are converted from American unit system to International unit system.

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".


To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest.


It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available.