Phenolic NP504 - Sheet

Alternative and trade names
NEMA GRADE: G-3, U.L. LISTED: N
Want to keep this datasheet? Save it now in your required format

Description

Woven glass fabric with high temperature phenolic resin. Good flexural, compressive and impact strengths at elevated temperatures. It is capable of continuous operation at 175°C. NP504 has excellent creep resistance because of the phenolic resin system. Meets MIL-I-24768/18 GPG. For NFPA 130 data please reference document NP504 Additional Data Sheet - NFPA 130.

This material data has been provided by Norplex Micarta.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bonding strength

23.0 °C

680.4 Kg

Show Supplier Material materials with Bonding strength of 680.4 Kg

ASTM D229, Condition A

Density

23.0 °C

1.8 g/cm³

Show Supplier Material materials with Density of 1.8 g/cm³

ASTM D792

Moisture absorption

23.0 °C

2 %

Show Supplier Material materials with Moisture absorption of 2 %

ASTM D570, Condition D₁-24/23

Mechanical

PropertyTemperatureValueComment

Compressive strength

23.0 °C

524 MPa

Show Supplier Material materials with Compressive strength of 524 MPa

ASTM D695, Condition A, Flatwise

Flexural modulus

23.0 °C

12.4 GPa

Show Supplier Material materials with Flexural modulus of 12.4 GPa

ASTM D790, Condition A

Flexural modulus, transverse

23.0 °C

9.7 GPa

Show Supplier Material materials with Flexural modulus, transverse of 9.7 GPa

ASTM D790, Condition A

Flexural strength

23.0 °C

379.2 MPa

Show Supplier Material materials with Flexural strength of 379.2 MPa

ASTM D790, Condition A

Flexural strength, transverse

23.0 °C

344.7 MPa

Show Supplier Material materials with Flexural strength, transverse of 344.7 MPa

ASTM D790, Condition A

Hardness, Rockwell M

23.0 °C

110 [-]

Show Supplier Material materials with Hardness, Rockwell M of 110 [-]

ASTM D785

Impact strength, Izod unnotched, ASTM

23.0 °C

641 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 641 J/m

ASTM D256, Condition E-48/50

Impact strength, Izod unnotched, ASTM, Transversal

23.0 °C

587 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM, Transversal of 587 J/m

ASTM D256, Condition E-48/50

Shear strength, transverse

23.0 °C

124.1 MPa

Show Supplier Material materials with Shear strength, transverse of 124.1 MPa

ASTM D732, Condition A

Tensile strength

23.0 °C

289.6 MPa

Show Supplier Material materials with Tensile strength of 289.6 MPa

ASTM D638, Condition A

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.5E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.5E-5 1/K

IPC-TM 650-2.4.24

Coefficient of thermal expansion, transverse

23.0 °C

1.8E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 1.8E-5 1/K

IPC-TM 650-2.4.24

Relative temperature index, electrical

140 °C

Show Supplier Material materials with Relative temperature index, electrical of 140 °C

UL Bulletin 746b¹

Relative temperature index, mechanical strength

170 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C

UL Bulletin 746b¹

Arc resistance

100 seconds, ASTM D495, Condition A

Flammability

UL Bulletin 94, Class HB

Electrical

PropertyTemperatureValueComment

Breakdown voltage

23.0 °C

40 - 55 kV

Show Supplier Material materials with Breakdown voltage of 40 - 55 kV

ASTM D149, Condition D-48/50 (Min.) & A (Max.)

Comparative tracking index

23.0 °C

150 V

Show Supplier Material materials with Comparative tracking index of 150 V

ASTM D3638

Dielectric strength

23.0 °C

22.83 - 23.62 kV/mm

Show Supplier Material materials with Dielectric strength of 22.83 - 23.62 kV/mm

ASTM D149, Condition D-48/50 (Min.) & A (Max.)

Technological properties

Property
Fillers

Glass Fabric

Other

1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use.

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".


To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest.