Epoxy RM511A - Rod

Alternative and trade names
NEMA GRADE: G-11 Type, U.L. LISTED: N
Want to keep this datasheet? Save it now in your required format

Description

Rolled and Molded Rods made from a glass fabric with a high temperature epoxy resin system. G-11 rods are not recognized by NEMA. However, they are recognized by the IEC Standard 61212: grade EP-GC-41. RM511A has equivalent electrical properties to G-10 rods, but with higher mechanical strength at elevated temperatures. Electrical properties are maintained in high humidity conditions. RM511A is not flame resistant.

This material data has been provided by Norplex Micarta.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.85 g/cm³

Show Supplier Material materials with Density of 1.85 g/cm³

ASTM D349

Moisture absorption

23.0 °C

0.08 %

Show Supplier Material materials with Moisture absorption of 0.08 %

ASTM D349, Condition D₁-24/23

Mechanical

PropertyTemperatureValueComment

Compressive strength

23.0 °C

507.45 MPa

Show Supplier Material materials with Compressive strength of 507.45 MPa

ASTM D349, Condition A

Flexural strength

23.0 °C

522.6 - 588.1 MPa

Show Supplier Material materials with Flexural strength of 522.6 - 588.1 MPa

ASTM D349, Condition T155 (Min.) & A (Max.)

Hardness, Rockwell M

23.0 °C

110 [-]

Show Supplier Material materials with Hardness, Rockwell M of 110 [-]

ASTM D349

Tensile strength

23.0 °C

385.42 MPa

Show Supplier Material materials with Tensile strength of 385.42 MPa

ASTM D349, Condition A

Thermal

PropertyValueComment

Relative temperature index, electrical

170 °C

Show Supplier Material materials with Relative temperature index, electrical of 170 °C

¹

Relative temperature index, mechanical strength

180 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 180 °C

¹

Flammability

UL 94, Class HB

Electrical

PropertyTemperatureValueComment

Dielectric constant, 1MHz

23.0 °C

4.3 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 4.3 [-]

ASTM D349, Condition A

Dielectric strength

23.0 °C

5.31 kV/mm

Show Supplier Material materials with Dielectric strength of 5.31 kV/mm

ASTM D349, Condition A

Dissipation factor, 1MHz

23.0 °C

4E-3 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 4E-3 [-]

ASTM D349, Condition A

Technological properties

Property
Fillers

Glass Fabric

Other

1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use


2.The mechanical properties are converted from American unit system to International unit system.

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".