Phenolic RT504F - Tube

Alternative and trade names
NEMA GRADE: G-3 Type, U.L. LISTED: N
Want to keep this datasheet? Save it now in your required format

Description

Grade RT504F is composed of a fine weave glass fabric combined with a phenolic resin system. It has excellent heat and chemical resistance in basic systems. It has good physical strength and high impact resistance. The use of a fine weave fabric is to provide better finish to the final part.

This material data has been provided by Norplex Micarta.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.78 g/cm³

Show Supplier Material materials with Density of 1.78 g/cm³

ASTM D792

Moisture absorption

23.0 °C

0.2 %

Show Supplier Material materials with Moisture absorption of 0.2 %

ASTM D570, Condition D₁-24/23

Mechanical

PropertyTemperatureValueComment

Compressive modulus

23.0 °C

7.69 MPa

Show Supplier Material materials with Compressive modulus of 7.69 MPa

Compressive strength

23.0 °C

296.47 MPa

Show Supplier Material materials with Compressive strength of 296.47 MPa

ASTM D695, Condition A

Hardness, Rockwell M

23.0 °C

120 [-]

Show Supplier Material materials with Hardness, Rockwell M of 120 [-]

ASTM D785

Tensile strength

23.0 °C

310.26 MPa

Show Supplier Material materials with Tensile strength of 310.26 MPa

ASTM D638, Condition A

Thermal

PropertyValueComment

Relative temperature index, electrical

180 °C

Show Supplier Material materials with Relative temperature index, electrical of 180 °C

¹

Relative temperature index, mechanical strength

160 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 160 °C

¹

Flammability

UL Bulletin 94, Class HB

Electrical

PropertyTemperatureValueComment

Dielectric strength

23.0 °C

15.74 - 16.53 kV/mm

Show Supplier Material materials with Dielectric strength of 15.74 - 16.53 kV/mm

ASTM D149, Condition D-48/50 (Min.) & A (Max.)

Technological properties

Property
Application areas

Typical applications include structural parts and can be substituted for G-7 in certain applications.

Fillers

Glass Fabric

Other

1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use


2.The mechanical properties are converted from American unit system to International unit system.

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".


To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest.


It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available.