Epoxy RT521M - Tube

Alternative and trade names
U.L. LISTED: N
Want to keep this datasheet? Save it now in your required format

Description

Medium weight glass fabric with epoxy resin system. RT521M combines excellent electrical characteristics with superior physical properties at cryogenic temperatures (-270 °C to 135 °C operating temperature range). Electrical properties maintained in high humidity conditions. RT521M is not flame resistant. RT521M is comparable sheet grade to Norplex-Micarta's sheet grade NP500CR.

This material data has been provided by Norplex Micarta.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.78 g/cm³

Show Supplier Material materials with Density of 1.78 g/cm³

ASTM D792

Moisture absorption

23.0 °C

0.05 %

Show Supplier Material materials with Moisture absorption of 0.05 %

ASTM D570, Condition D₁-24/23

Mechanical

PropertyTemperatureValueComment

Compressive modulus

23.0 °C

7.58 MPa

Show Supplier Material materials with Compressive modulus of 7.58 MPa

ASTM D695, Condition A

Compressive strength

23.0 °C

320.61 MPa

Show Supplier Material materials with Compressive strength of 320.61 MPa

ASTM D695, Condition A

Hardness, Rockwell M

23.0 °C

110 [-]

Show Supplier Material materials with Hardness, Rockwell M of 110 [-]

ASTM D785

Tensile strength

23.0 °C

310.26 MPa

Show Supplier Material materials with Tensile strength of 310.26 MPa

ASTM D638, Condition A

Thermal

PropertyValueComment

Relative temperature index, electrical

130 °C

Show Supplier Material materials with Relative temperature index, electrical of 130 °C

¹

Relative temperature index, mechanical strength

135 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 135 °C

¹

Flammability

UL Bulletin 94, Class HB

Electrical

PropertyTemperatureValueComment

Breakdown voltage

23.0 °C

85 kV

Show Supplier Material materials with Breakdown voltage of 85 kV

ASTM D149, Condition A

Dielectric strength

23.0 °C

19.68 - 23.62 kV/mm

Show Supplier Material materials with Dielectric strength of 19.68 - 23.62 kV/mm

ASTM D149, Condition D-48/50 (Min.) & A (Max.)

Technological properties

Property
Fillers

Glass Fabric

Other

1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use


2.The mechanical properties are converted from American unit system to International unit system.

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".


To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest.


It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available.