Phenolic NP504WR - Sheet

Alternative and trade names
U.L. LISTED: N
Want to keep this datasheet? Save it now in your required format

Description

NP504WR is a phenolic resin combined with a heavy weight glass fabric, 24 or 30 oz depending on the application and machining requirements.

This material data has been provided by Norplex Micarta.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bonding strength

23.0 °C

181.44 Kg

Show Supplier Material materials with Bonding strength of 181.44 Kg

Condition A

Density

23.0 °C

2.18 g/cm³

Show Supplier Material materials with Density of 2.18 g/cm³

Moisture absorption

23.0 °C

1.4 %

Show Supplier Material materials with Moisture absorption of 1.4 %

Mechanical

PropertyTemperatureValueComment

Compressive strength

23.0 °C

269 - 448.1 MPa

Show Supplier Material materials with Compressive strength of 269 - 448.1 MPa

Condition A, Flatwise (Max.) & Edgewise (Min.)

Flexural strength

23.0 °C

159.96 MPa

Show Supplier Material materials with Flexural strength of 159.96 MPa

Condition A

Flexural strength, transverse

23.0 °C

118.59 MPa

Show Supplier Material materials with Flexural strength, transverse of 118.59 MPa

Condition A

Hardness, Rockwell M

23.0 °C

110 [-]

Show Supplier Material materials with Hardness, Rockwell M of 110 [-]

Impact strength, Izod notched, ASTM

23.0 °C

800.7 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 800.7 J/m

Condition E-48/50

Impact strength, Izod notched, ASTM, Transversal

23.0 °C

800.7 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM, Transversal of 800.7 J/m

Condition E-48/50

Tensile strength

23.0 °C

434.37 MPa

Show Supplier Material materials with Tensile strength of 434.37 MPa

Condition A

Tensile strength, transverse

23.0 °C

268.9 MPa

Show Supplier Material materials with Tensile strength, transverse of 268.9 MPa

Condition A

Thermal

PropertyValue

Flammability

UL 94, Class V-0

Technological properties

Property
Application areas

NP504WR is designed for structural applications.

Fillers

Glass Fabric

Other

The mechanical properties are converted from American unit system to International unit system.

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".


To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest.


It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available.