Phenolic MC514MG - Sheet

Alternative and trade names
U.L. LISTED: N
Want to keep this datasheet? Save it now in your required format

Description

MC514MG is a glass phenolic, semi-conductive laminate which was designed for corona discharge in the power generation industry. The graphitic carbon additive in the resin system enables easy installation in the slots and provides the necessary conductivity to safely remove harmful charges from the system.

This material data has been provided by Norplex Micarta.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bonding strength

23.0 °C

499 Kg

Show Supplier Material materials with Bonding strength of 499 Kg

ASTM D229, Condition A

Density

23.0 °C

1.8 g/cm³

Show Supplier Material materials with Density of 1.8 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Compressive strength

23.0 °C

330.9 MPa

Show Supplier Material materials with Compressive strength of 330.9 MPa

ASTM D695, Condition A, Flatwise

Flexural strength

23.0 °C

234.4 MPa

Show Supplier Material materials with Flexural strength of 234.4 MPa

ASTM D790, Condition A

Flexural strength, transverse

23.0 °C

172.4 MPa

Show Supplier Material materials with Flexural strength, transverse of 172.4 MPa

ASTM D790, Condition A

Hardness, Rockwell M

23.0 °C

110 [-]

Show Supplier Material materials with Hardness, Rockwell M of 110 [-]

ASTM D785

Thermal

PropertyValueComment

Relative temperature index, mechanical strength

155 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 155 °C

UL Bulletin 746b¹

Electrical

PropertyTemperatureValueComment

Surface resistivity

23.0 °C

400 - 20000 Ω/sq

Show Supplier Material materials with Surface resistivity of 400 - 20000 Ω/sq

ASTM D257

Technological properties

Property
Fillers

Glass Fabric

Other

1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use.

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".


To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest.


It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available.