Being a heat treated version of RT310, RT310H is a tube made from a medium weight canvas fabric combined with a phenolic resin that has good physical properties and machining characteristics. RT310H also complies with MIL-I-24768/16, Type FBM and ASTM D709 Type II Grade C.
Density
ρ1.3 g/cm³ at 23 °C
ASTM D792
Moisture absorption
cmoisture1.8 % at 23 °C
ASTM D570, Condition Dᵢ-24/23
Flammability
UL Bulletin 94, Class HB, Condition A
Relative temperature index, electrical
RTIel140 °C
¹
Relative temperature index, mechanical strength
RTIstr140 °C
¹
Dielectric strength
EDS5.9 kV/mm at 23 °C
ASTM D149, Condition A
Application areas
Typical applications include textile bobbins, lap spools and structural parts that require good impact strength.
Fillers
Cotton Fabric
Other
1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use
2.The mechanical properties are converted from American unit system to International unit system.
Supplier Disclaimer
This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".
To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest.
It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available.
This material data has been provided by Norplex Micarta.