Description

Fine weave canvas phenolic engineered for dimensional stability and mechanical strength at temperatures as high as 125oC. Providing excellent moisture resistance and easy to machine, NP342LS low- shrink material was designed for use in Class B generators for wedge applications and can be tested to the General Electric specification A50A341.

Related Standards

This material data has been provided by Norplex Micarta.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.37 g/cm³

Show Supplier Material materials with Density of 1.37 g/cm³

ASTM D792

Moisture absorption

23.0 °C

0.58 %

Show Supplier Material materials with Moisture absorption of 0.58 %

ASTM D570, Condition Dᵢ-24/23

Mechanical

PropertyTemperatureValueComment

Compressive strength

23.0 °C

282.7 MPa

Show Supplier Material materials with Compressive strength of 282.7 MPa

ASTM D695, Condition A, Flatwise

Elastic modulus

23.0 °C

9.7 GPa

Show Supplier Material materials with Elastic modulus of 9.7 GPa

ASTM D638, Condition A

Elastic modulus, transverse

23.0 °C

10.5 GPa

Show Supplier Material materials with Elastic modulus, transverse of 10.5 GPa

ASTM D638, Condition A

Flexural strength

23.0 °C

144.1 MPa

Show Supplier Material materials with Flexural strength of 144.1 MPa

ASTM D790, Condition A

Flexural strength, transverse

23.0 °C

146.2 MPa

Show Supplier Material materials with Flexural strength, transverse of 146.2 MPa

ASTM D790, Condition A

Hardness, Rockwell M

23.0 °C

95 [-]

Show Supplier Material materials with Hardness, Rockwell M of 95 [-]

ASTM D785

Impact strength, Izod unnotched, ASTM

23.0 °C

133 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 133 J/m

ASTM D256, Condition E-48/50

Impact strength, Izod unnotched, ASTM, Transversal

23.0 °C

155 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM, Transversal of 155 J/m

ASTM D256, Condition E-48/50

Shear strength, transverse

23.0 °C

148.2 MPa

Show Supplier Material materials with Shear strength, transverse of 148.2 MPa

ASTM D732, Condition A

Tensile strength

23.0 °C

91 MPa

Show Supplier Material materials with Tensile strength of 91 MPa

ASTM D638, Condition A

Tensile strength, transverse

23.0 °C

102 MPa

Show Supplier Material materials with Tensile strength, transverse of 102 MPa

ASTM D638, Condition A

Thermal

PropertyValueComment

Relative temperature index, electrical

125 °C

Show Supplier Material materials with Relative temperature index, electrical of 125 °C

UL Bulletin 746b¹

Relative temperature index, mechanical strength

125 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 125 °C

UL Bulletin 746b¹

Flammability

UL Bulletin 94, Class HB, Condition A

Electrical

PropertyTemperatureValueComment

Breakdown voltage

23.0 °C

64 kV

Show Supplier Material materials with Breakdown voltage of 64 kV

ASTM D149, Condition A

Dielectric constant, 1MHz

23.0 °C

5.17 - 5.35 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 5.17 - 5.35 [-]

ASTM D150, Condition A (Min.) & D-24/23 (Max.)

Dissipation factor, 1MHz

23.0 °C

0.07 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 0.07 [-]

ASTM D150, Condition A (Min.) & D-24/23 (Max.)

Technological properties

Property
Fillers

Cotton Fabric

Other

1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use.

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".


To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest.


It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available.