Epoxy RM326 - Rod

Alternative and trade names
NEMA GRADE: L, U.L. LISTED: N
Want to keep this datasheet? Save it now in your required format

Description

Rolled and Molded Rods made from a fine weave (linen) cotton fabric impregnated with an epoxy resin system.

This material data has been provided by Norplex Micarta.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.35 g/cm³

Show Supplier Material materials with Density of 1.35 g/cm³

ASTM D349

Moisture absorption

23.0 °C

0.51 %

Show Supplier Material materials with Moisture absorption of 0.51 %

ASTM D349

Mechanical

PropertyTemperatureValueComment

Compressive strength

23.0 °C

206.15 MPa

Show Supplier Material materials with Compressive strength of 206.15 MPa

ASTM D349, Condition A

Flexural strength

23.0 °C

151.68 MPa

Show Supplier Material materials with Flexural strength of 151.68 MPa

ASTM D349, Condition A

Hardness, Rockwell M

23.0 °C

100 [-]

Show Supplier Material materials with Hardness, Rockwell M of 100 [-]

ASTM D349

Tensile strength

23.0 °C

103.42 MPa

Show Supplier Material materials with Tensile strength of 103.42 MPa

ASTM D349, Condition A

Thermal

PropertyValueComment

Relative temperature index, electrical

115 °C

Show Supplier Material materials with Relative temperature index, electrical of 115 °C

¹

Relative temperature index, mechanical strength

125 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 125 °C

¹

Flammability

UL 94, Class HB, Condition A

Technological properties

Property
Application areas

RM326 is used for electrical and mechanical applications, meeting NEMA L or LE requirements.

Fillers

Cotton Fabric

Other

1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use


2.The mechanical properties are converted from American unit system to International unit system.

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".