Phenolic NP313 - Sheet

Alternative and trade names
U.L. LISTED: N
Want to keep this datasheet? Save it now in your required format

Description

Canvas phenolic laminate with molybdenum disulfide lubricant. The mechanical properties are slightly lower than NP310. NP313 is used for lubricity in the composite when carbon (graphite) cannot be used because of conductivity.

This material data has been provided by Norplex Micarta.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bonding strength

23.0 °C

861.8 Kg

Show Supplier Material materials with Bonding strength of 861.8 Kg

ASTM D229, Condition A

Density

23.0 °C

1.4 g/cm³

Show Supplier Material materials with Density of 1.4 g/cm³

ASTM D792

Moisture absorption

23.0 °C

1.95 %

Show Supplier Material materials with Moisture absorption of 1.95 %

ASTM D570, Condition D₁-24/23

Mechanical

PropertyTemperatureValueComment

Compressive strength

23.0 °C

248.2 MPa

Show Supplier Material materials with Compressive strength of 248.2 MPa

ASTM D695, Condition A

Flexural modulus

23.0 °C

8.3 GPa

Show Supplier Material materials with Flexural modulus of 8.3 GPa

ASTM D790, Condition A

Flexural modulus, transverse

23.0 °C

6.9 GPa

Show Supplier Material materials with Flexural modulus, transverse of 6.9 GPa

ASTM D790, Condition A

Flexural strength

23.0 °C

131 MPa

Show Supplier Material materials with Flexural strength of 131 MPa

ASTM D349, Condition A

Flexural strength, transverse

23.0 °C

117.2 MPa

Show Supplier Material materials with Flexural strength, transverse of 117.2 MPa

ASTM D349, Condition A

Hardness, Rockwell M

23.0 °C

100 [-]

Show Supplier Material materials with Hardness, Rockwell M of 100 [-]

ASTM D785

Impact strength, Izod unnotched, ASTM

23.0 °C

91 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 91 J/m

ASTM D256, Condition E-48/50

Impact strength, Izod unnotched, ASTM, Transversal

23.0 °C

75 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM, Transversal of 75 J/m

ASTM D256, Condition E-48/50

Shear strength, transverse

23.0 °C

93.1 MPa

Show Supplier Material materials with Shear strength, transverse of 93.1 MPa

ASTM D732, Condition A

Tensile strength

23.0 °C

75.8 MPa

Show Supplier Material materials with Tensile strength of 75.8 MPa

ASTM D638, Condition A

Tensile strength, transverse

23.0 °C

62.1 MPa

Show Supplier Material materials with Tensile strength, transverse of 62.1 MPa

ASTM D638, Condition A

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.8E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.8E-5 1/K

IPC-TM 650-2.4.24

Coefficient of thermal expansion, transverse

23.0 °C

2.4E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 2.4E-5 1/K

IPC-TM 650-2.4.24

Relative temperature index, mechanical strength

145 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 145 °C

UL Bulletin 746b¹

Flammability

UL Bulletin 94, Class HB, Condition A

Technological properties

Property
Fillers

Cotton Fabric and MoS2

Other

1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use.

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".