Phenolic NP324FR - Sheet

Alternative and trade names
U.L. LISTED: N
Want to keep this datasheet? Save it now in your required format

Description

NP324FR is a fine weave cotton fabric which has been bleached to remove impurities, and a modified phenolic resin with powdered PTFE added for lubrication as well as a flame retardant. It has low moisture absorption and excellent dimensional stability. NP324FR provides excellent machining characteristics.

This material data has been provided by Norplex Micarta.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bonding strength

23.0 °C

1150 - 1230 Kg

Show Supplier Material materials with Bonding strength of 1150 - 1230 Kg

Condition A (Max.) & D-48/50 (Min.)

Moisture absorption

23.0 °C

1.51 %

Show Supplier Material materials with Moisture absorption of 1.51 %

Condition Dᵢ-24/23

Mechanical

PropertyTemperatureValueComment

Flexural strength

23.0 °C

172.37 MPa

Show Supplier Material materials with Flexural strength of 172.37 MPa

Condition A

Flexural strength, transverse

23.0 °C

144.79 MPa

Show Supplier Material materials with Flexural strength, transverse of 144.79 MPa

Condition A

Impact strength, Izod notched, ASTM

23.0 °C

117.43 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 117.43 J/m

Condition E-48/50

Impact strength, Izod notched, ASTM, Transversal

23.0 °C

106.76 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM, Transversal of 106.76 J/m

Condition E-48/50

Thermal

PropertyValue

Flammability

UL 94, Class HB

Electrical

PropertyTemperatureValueComment

Breakdown voltage

23.0 °C

60 kV

Show Supplier Material materials with Breakdown voltage of 60 kV

Condition A

Technological properties

Property
Fillers

Cotton Fabric and PTFE

Other

1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use


2.The mechanical properties are converted from American unit system to International unit system.

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".


To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest.


It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available.