General
Property | Value | Temperature | Comment |
---|---|---|---|
Density | 1.39 g/cm³ Show Supplier Material materials with Density of 1.39 g/cm³ at 23.0 °C | 23.0 °C | ASTM D349 |
Moisture absorption | 2.2 % Show Supplier Material materials with Moisture absorption of 2.2 % at 23.0 °C | 23.0 °C | ASTM D349, Condition Dᵢ-24/23 |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Compressive strength | 196.5 MPa Show Supplier Material materials with Compressive strength of 196.5 MPa at 23.0 °C | 23.0 °C | ASTM D349, Condition A |
Flexural strength | 124.11 MPa Show Supplier Material materials with Flexural strength of 124.11 MPa at 23.0 °C | 23.0 °C | ASTM D349, Condition A |
Hardness, Rockwell M | 89 [-] Show Supplier Material materials with Hardness, Rockwell M of 89 [-] at 23.0 °C | 23.0 °C | ASTM D349, Condition A |
Tensile strength | 63.43 MPa Show Supplier Material materials with Tensile strength of 63.43 MPa at 23.0 °C | 23.0 °C | ASTM D349, Condition A |
Thermal
Property | Value | Comment |
---|---|---|
Flammability | UL Bulletin 94, Class V-1, Condition A | |
Relative temperature index, electrical | 115 °C Show Supplier Material materials with Relative temperature index, electrical of 115 °C | ¹ |
Relative temperature index, mechanical strength | 125 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 125 °C | ¹ |
Technological properties
Property | ||
---|---|---|
Application areas | RM329 is used for decorative application simulating the color of Ivory. | |
Fillers | Cotton Fabric | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use 2.The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |