Description

NP338 is a combination of two Norplex-Micarta grades, NP310 which is a canvas phenolic, on one side of the laminate, and NP315, a canvas phenolic with graphite added as a solid lubricant on the other side of the laminate. Material is conductive to electricity and should not be used where conductivity is detrimental to the application.

This material data has been provided by Norplex Micarta.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.42 g/cm³

Show Supplier Material materials with Density of 1.42 g/cm³

ASTM D792

Moisture absorption

23.0 °C

1.78 %

Show Supplier Material materials with Moisture absorption of 1.78 %

ASTM D570, Condition D₁-24/23

Mechanical

PropertyTemperatureValueComment

Compressive strength

23.0 °C

270.3 MPa

Show Supplier Material materials with Compressive strength of 270.3 MPa

ASTM D695, Condition A, Flatwise

Elastic modulus

23.0 °C

10.2 GPa

Show Supplier Material materials with Elastic modulus of 10.2 GPa

ASTM D638, Condition A

Elastic modulus, transverse

23.0 °C

9.9 GPa

Show Supplier Material materials with Elastic modulus, transverse of 9.9 GPa

ASTM D638, Condition A

Flexural modulus

23.0 °C

6.8 GPa

Show Supplier Material materials with Flexural modulus of 6.8 GPa

ASTM D790, Condition A

Flexural modulus, transverse

23.0 °C

6.6 GPa

Show Supplier Material materials with Flexural modulus, transverse of 6.6 GPa

ASTM D790, Condition A

Flexural strength

23.0 °C

145.5 MPa

Show Supplier Material materials with Flexural strength of 145.5 MPa

ASTM D790, Condition A

Flexural strength, transverse

23.0 °C

131 MPa

Show Supplier Material materials with Flexural strength, transverse of 131 MPa

ASTM D790, Condition A

Hardness, Rockwell M

23.0 °C

86 [-]

Show Supplier Material materials with Hardness, Rockwell M of 86 [-]

ASTM D785

Impact strength, Izod unnotched, ASTM

23.0 °C

224 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 224 J/m

ASTM D256, Condition E-48/50

Impact strength, Izod unnotched, ASTM, Transversal

23.0 °C

181 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM, Transversal of 181 J/m

ASTM D256, Condition E-48/50

Shear strength, transverse

23.0 °C

140.7 MPa

Show Supplier Material materials with Shear strength, transverse of 140.7 MPa

ASTM D732, Condition A

Tensile strength

23.0 °C

95.8 MPa

Show Supplier Material materials with Tensile strength of 95.8 MPa

ASTM D638, Condition A

Tensile strength, transverse

23.0 °C

79.3 MPa

Show Supplier Material materials with Tensile strength, transverse of 79.3 MPa

ASTM D638, Condition A

Thermal

PropertyValue

Flammability

UL 94, Class HB, Condition A

Technological properties

Property
Application areas

NP338 is ideal for applications requiring high impact strength and low coefficient of friction such as railway couplers.

Fillers

Cotton Fabric and Graphite Powder

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".


To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest.


It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available.