Description

Grade BT18NPM is a tube made from a HEAVY weight canvas fabric combined with a phenolic resin that has good physical properties and machining characteristics.

This material data has been provided by Norplex Micarta.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.34 g/cm³

Show Supplier Material materials with Density of 1.34 g/cm³

ASTM D792

Moisture absorption

23.0 °C

1.3 %

Show Supplier Material materials with Moisture absorption of 1.3 %

ASTM D570, Condition Dᵢ-24/23

Mechanical

PropertyTemperatureValueComment

Compressive modulus

23.0 °C

2.41 MPa

Show Supplier Material materials with Compressive modulus of 2.41 MPa

ASTM D695, Condition A

Compressive strength

23.0 °C

127.55 MPa

Show Supplier Material materials with Compressive strength of 127.55 MPa

ASTM D695, Condition A

Hardness, Rockwell M

23.0 °C

80 [-]

Show Supplier Material materials with Hardness, Rockwell M of 80 [-]

ASTM D785

Tensile strength

23.0 °C

37.92 MPa

Show Supplier Material materials with Tensile strength of 37.92 MPa

ASTM D638, Condition A

Thermal

PropertyValueComment

Relative temperature index, mechanical strength

140 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C

¹

Flammability

UL Bulletin 94, Class HB, Condition A

Technological properties

Property
Application areas

Typical applications include journal bearings and structural parts that require good impact strength and wear resistance.

Fillers

Cotton Fabric

Other

1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use


2.The mechanical properties are converted from American unit system to International unit system.

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".


To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest.


It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available.