Phenolic BP11HPN - Sheet

Alternative and trade names
U.L. LISTED: N
Want to keep this datasheet? Save it now in your required format

Description

Canvas machining grade for structural and mechanical applications. BP11HPN has better impact strength than phenolic paper grades.

This material data has been provided by Norplex Micarta.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bonding strength

23.0 °C

1088 Kg

Show Supplier Material materials with Bonding strength of 1088 Kg

ASTM D229, Condition A

Density

23.0 °C

1.37 g/cm³

Show Supplier Material materials with Density of 1.37 g/cm³

ASTM D792

Moisture absorption

23.0 °C

0.8 - 3.4 %

Show Supplier Material materials with Moisture absorption of 0.8 - 3.4 %

ASTM D570, depending on speciemen thickness

Mechanical

PropertyTemperatureValueComment

Compressive strength

23.0 °C

241.3 MPa

Show Supplier Material materials with Compressive strength of 241.3 MPa

ASTM D695, Condition A, Flatwise

Flexural modulus

23.0 °C

17.2 GPa

Show Supplier Material materials with Flexural modulus of 17.2 GPa

ASTM D790, Condition A

Flexural modulus, transverse

23.0 °C

16.5 GPa

Show Supplier Material materials with Flexural modulus, transverse of 16.5 GPa

ASTM D790, Condition A

Flexural strength

23.0 °C

124.1 MPa

Show Supplier Material materials with Flexural strength of 124.1 MPa

ASTM D790, Condition A

Flexural strength, transverse

23.0 °C

124.1 MPa

Show Supplier Material materials with Flexural strength, transverse of 124.1 MPa

ASTM D790, Condition A

Hardness, Rockwell M

23.0 °C

100 [-]

Show Supplier Material materials with Hardness, Rockwell M of 100 [-]

ASTM D785

Impact strength, Izod unnotched, ASTM

23.0 °C

125 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 125 J/m

ASTM D256, Condition E-48/50

Impact strength, Izod unnotched, ASTM, Transversal

23.0 °C

108 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM, Transversal of 108 J/m

ASTM D256, Condition E-48/50

Thermal

PropertyValueComment

Relative temperature index, electrical

125 °C

Show Supplier Material materials with Relative temperature index, electrical of 125 °C

UL Bulletin 746b¹

Relative temperature index, mechanical strength

125 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 125 °C

UL Bulletin 746b¹

Flammability

UL Bulletin 94, Class HB, Condition A

Electrical

PropertyTemperatureValueComment

Breakdown voltage

23.0 °C

55 kV

Show Supplier Material materials with Breakdown voltage of 55 kV

ASTM D149, Condition A

Dielectric strength

23.0 °C

20.75 kV/mm

Show Supplier Material materials with Dielectric strength of 20.75 kV/mm

ASTM D149, Condition A

Technological properties

Property
Application areas

Structural and mechanical applications

Fillers

Cotton Fabric

Other

1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".