BP11NPN is a canvas machining grade for structural and mechanical applications. It has better impact strength than phenolic paper grades.
Bonding strength
Fbond1134 Kg at 23 °C
ASTM D229, Condition A
Density
ρ1.37 g/cm³ at 23 °C
ASTM D792
Moisture absorption
cmoisture3.5 % at 23 °C
ASTM D570, Condition Dᵢ-24/23
Arc resistance
15 seconds, ASTM D495, Condition A
Coefficient of thermal expansion
α2E-5 1/K at 23 °C
IPC-TM 650-2.4.24
Coefficient of thermal expansion, transverse
αtrans2.2E-5 1/K at 23 °C
IPC-TM 650-2.4.24
Flammability
UL Bulletin 94, Class HB, Condition A
Relative temperature index, electrical
RTIel115 °C
UL Bulletin 746b¹
Relative temperature index, mechanical strength
RTIstr125 °C
UL Bulletin 746b¹
Breakdown voltage
Ubreak5 - 20 kV at 23 °C
ASTM D149, Condition D48/50 (Min.) & A (Max.)
Comparative tracking index
CTI155 V at 23 °C
ASTM D3638
Dielectric strength
EDS5.91 - 15.75 kV/mm at 23 °C
ASTM D149, Condition D-48/50 (Min.) & A (Max.)
Application areas
Structural and mechanical applications
Fillers
Cotton Fabric
Other
1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use
Supplier Disclaimer
This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".
To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest.
It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available.
This material data has been provided by Norplex Micarta.