Phenolic BP81NPN - Sheet

Alternative and trade names
U.L. LISTED: N
Want to keep this datasheet? Save it now in your required format

Description

BP81NPN is a cotton phenolic composite which is specifically designed to dissipate heat better than standard cotton phenolic products.

This material data has been provided by Norplex Micarta.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bonding strength

23.0 °C

544.3 Kg

Show Supplier Material materials with Bonding strength of 544.3 Kg

ASTM D229, Condition A

Density

23.0 °C

1.47 g/cm³

Show Supplier Material materials with Density of 1.47 g/cm³

ASTM D792

Moisture absorption

23.0 °C

2.5 %

Show Supplier Material materials with Moisture absorption of 2.5 %

ASTM D570, Condition Dᵢ-24/23

Mechanical

PropertyTemperatureValueComment

Compressive strength

23.0 °C

296.5 MPa

Show Supplier Material materials with Compressive strength of 296.5 MPa

ASTM D695, Condition A, Flatwise

Hardness, Rockwell M

23.0 °C

100 [-]

Show Supplier Material materials with Hardness, Rockwell M of 100 [-]

ASTM D785

Tensile strength

23.0 °C

296.5 MPa

Show Supplier Material materials with Tensile strength of 296.5 MPa

ASTM D638, Condition A

Thermal

PropertyValueComment

Relative temperature index, mechanical strength

150 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 150 °C

¹

Flammability

UL Bulletin 94, Class HB, Condition A

Technological properties

Property
Application areas

Applications include trunion wheels, wire strander rolls and pile-driver head cushions.

Fillers

Cotton Fabric

Other

1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".