Phenolic NP629 - Sheet

Alternative and trade names
NEMA GRADE: XX, U.L. LISTED: N
Want to keep this datasheet? Save it now in your required format

Description

NP629 is a paper-phenolic high-pressure laminate and intended primarily for mechanical applications, but is suitable for electrical applications as well. The electrical properties are not quite as good as those of NP630.

This material data has been provided by Norplex Micarta.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bonding strength

23.0 °C

408.2 Kg

Show Supplier Material materials with Bonding strength of 408.2 Kg

ASTM D229, Condition A

Density

23.0 °C

1.35 g/cm³

Show Supplier Material materials with Density of 1.35 g/cm³

ASTM D792

Moisture absorption

23.0 °C

2 %

Show Supplier Material materials with Moisture absorption of 2 %

ASTM D570, Condition Dᵢ-24/23

Mechanical

PropertyTemperatureValueComment

Compressive strength

23.0 °C

172.4 MPa

Show Supplier Material materials with Compressive strength of 172.4 MPa

ASTM D695, Condition A, Flatwise

Flexural strength

23.0 °C

151.7 MPa

Show Supplier Material materials with Flexural strength of 151.7 MPa

ASTM D790, Condition A

Flexural strength, transverse

23.0 °C

117.2 MPa

Show Supplier Material materials with Flexural strength, transverse of 117.2 MPa

ASTM D790, Condition A

Hardness, Rockwell M

23.0 °C

95 [-]

Show Supplier Material materials with Hardness, Rockwell M of 95 [-]

ASTM D785

Impact strength, Izod unnotched, ASTM

23.0 °C

27 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 27 J/m

ASTM D256, Condition E-48/50

Impact strength, Izod unnotched, ASTM, Transversal

23.0 °C

21 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM, Transversal of 21 J/m

ASTM D256, Condition E-48/50

Shear strength, transverse

23.0 °C

79.3 MPa

Show Supplier Material materials with Shear strength, transverse of 79.3 MPa

ASTM D732, Condition A

Tensile strength

23.0 °C

93.1 MPa

Show Supplier Material materials with Tensile strength of 93.1 MPa

ASTM D638, Condition A

Tensile strength, transverse

23.0 °C

79.3 MPa

Show Supplier Material materials with Tensile strength, transverse of 79.3 MPa

ASTM D638, Condition A

Thermal

PropertyValueComment

Relative temperature index, electrical

130 °C

Show Supplier Material materials with Relative temperature index, electrical of 130 °C

UL Bulletin 746b¹

Relative temperature index, mechanical strength

130 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C

UL Bulletin 746b¹

Flammability

UL Bulletin 94, Class HB, Condition A

Electrical

PropertyTemperatureValueComment

Breakdown voltage

23.0 °C

5 - 40 kV

Show Supplier Material materials with Breakdown voltage of 5 - 40 kV

ASTM D149, Condition D48/50 (Min.) & A (Max.)

Dielectric constant, 1MHz

23.0 °C

6.2 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 6.2 [-]

ASTM D150, Condition D-24/23

Dissipation factor, 1MHz

23.0 °C

0.05 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 0.05 [-]

ASTM D150, Condition D-24/23

Technological properties

Property
Application areas

It is used for mechanical and electrical applications.

Fillers

Paper

Other

1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".


To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest.


It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available.