A paper-base laminate with low phenolic resin content for hard, flat surfaces.

This material data has been provided by Norplex Micarta.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.3 g/cm³

Show Supplier Material materials with Density of 1.3 g/cm³

ASTM D792

Moisture absorption

23.0 °C

8 %

Show Supplier Material materials with Moisture absorption of 8 %

ASTM D570, Condition Dᵢ-24/23

Mechanical

PropertyTemperatureValueComment

Compressive strength

23.0 °C

241.3 MPa

Show Supplier Material materials with Compressive strength of 241.3 MPa

ASTM D695, Condition A, Flatwise

Flexural strength

23.0 °C

172.4 MPa

Show Supplier Material materials with Flexural strength of 172.4 MPa

ASTM D790, Condition A

Flexural strength, transverse

23.0 °C

172.4 MPa

Show Supplier Material materials with Flexural strength, transverse of 172.4 MPa

ASTM D790, Condition A

Hardness, Rockwell M

23.0 °C

90 [-]

Show Supplier Material materials with Hardness, Rockwell M of 90 [-]

ASTM D785

Impact strength, Izod unnotched, ASTM

23.0 °C

29 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 29 J/m

ASTM D256, Condition E-48/50

Impact strength, Izod unnotched, ASTM, Transversal

23.0 °C

27 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM, Transversal of 27 J/m

ASTM D256, Condition E-48/50

Tensile strength

23.0 °C

117.2 MPa

Show Supplier Material materials with Tensile strength of 117.2 MPa

ASTM D638, Condition A

Tensile strength, transverse

23.0 °C

89.6 MPa

Show Supplier Material materials with Tensile strength, transverse of 89.6 MPa

ASTM D638, Condition A

Thermal

PropertyValueComment

Relative temperature index, mechanical strength

150 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 150 °C

UL Bulletin 746b¹

Flammability

UL Bulletin 94, Class HB, Condition A

Technological properties

Property
Application areas

This material is normally used in the printed circuit board industry as a backup for the drilling operation. However, it is also used in other industries for tooling stock because of its ease of machining and good dimensional stability.

Fillers

Paper

Other

1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".


To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest.


It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available.