1.4112

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by Remy Stahl.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Chemical properties

Property

Carbon

0.85 - 0.95 %

Chromium

17 - 19 %

Iron

Balance

Manganese

1 %

max.

Molybdenum

0.9 - 1.3 %

Phosphorus

0.04 %

max.

Silicon

1 %

max.

Sulfur

0.015 %

max.

Vanadium

0.07 - 0.12 %

Technological properties

Property
Application areas

Apparatus engineering, shipbuilding, wear parts, perforated (Break) discs, balance pan and scale cutting, professional knives, high-quality cutting surgical instruments, rolling bearings, screw elements, spray nozzles

Processing history

Annealed