1.4961

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by Remy Stahl.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 10-125 mm

Mechanical

PropertyValue

Tensile strength

510.0 - 690.0 MPa

Show Supplier Material materials with Tensile strength of 510.0 - 690.0 MPa

Chemical properties

PropertyValueComment

Aluminium

0.35 %

Show Supplier Material materials with Aluminium of 0.35 %

max.

Boron

0.003 - 0.01 %

Show Supplier Material materials with Boron of 0.003 - 0.01 %

Carbon

0.08 %

Show Supplier Material materials with Carbon of 0.08 %

max.

Chromium

13.5 - 16.0 %

Show Supplier Material materials with Chromium of 13.5 - 16.0 %

Manganese

2.0 %

Show Supplier Material materials with Manganese of 2.0 %

max.

Molybdenum

1.0 - 1.8 %

Show Supplier Material materials with Molybdenum of 1.0 - 1.8 %

Nickel

24.0 - 27.0 %

Show Supplier Material materials with Nickel of 24.0 - 27.0 %

Phosphorus

0.025 %

Show Supplier Material materials with Phosphorus of 0.025 %

max.

Silicon

1.0 %

Show Supplier Material materials with Silicon of 1.0 %

max.

Sulfur

0.015 %

Show Supplier Material materials with Sulfur of 0.015 %

max.

Titanium

1.9 - 2.3 %

Show Supplier Material materials with Titanium of 1.9 - 2.3 %

Vanadium

0.1 - 0.5 %

Show Supplier Material materials with Vanadium of 0.1 - 0.5 %

Technological properties

Property
Application areas

Mechanical Engineering, Apparatus engineering, Components for thermal power plants like valves, discs, housings, superheaters and steam line pipes

Processing history

Solution Annealed