Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 20-320 mm

Mechanical

PropertyValueComment

Elongation

12 %

Show Supplier Material materials with Elongation of 12 %

min.

Tensile strength

700.0 - 850.0 MPa

Show Supplier Material materials with Tensile strength of 700.0 - 850.0 MPa

Yield strength

500.0 MPa

Show Supplier Material materials with Yield strength of 500.0 MPa

min., RP02

Chemical properties

PropertyValueComment

Aluminium

0.02 %

Show Supplier Material materials with Aluminium of 0.02 %

max.

Boron

0.0015 %

Show Supplier Material materials with Boron of 0.0015 %

Carbon

0.17 - 0.23 %

Show Supplier Material materials with Carbon of 0.17 - 0.23 %

max.

Chromium

10.0 - 11.5 %

Show Supplier Material materials with Chromium of 10.0 - 11.5 %

Manganese

0.4 - 0.9 %

Show Supplier Material materials with Manganese of 0.4 - 0.9 %

Molybdenum

0.5 - 0.8 %

Show Supplier Material materials with Molybdenum of 0.5 - 0.8 %

Nickel

0.2 - 0.6 %

Show Supplier Material materials with Nickel of 0.2 - 0.6 %

Niobium

0.25 - 0.55 %

Show Supplier Material materials with Niobium of 0.25 - 0.55 %

Nitrogen

0.05 - 0.1 %

Show Supplier Material materials with Nitrogen of 0.05 - 0.1 %

Phosphorus

0.03 %

Show Supplier Material materials with Phosphorus of 0.03 %

max.

Silicon

0.5 %

Show Supplier Material materials with Silicon of 0.5 %

max.

Sulfur

0.015 %

Show Supplier Material materials with Sulfur of 0.015 %

max.

Vanadium

0.1 - 0.3 %

Show Supplier Material materials with Vanadium of 0.1 - 0.3 %

Technological properties

Property
Application areas

Power plant engineering, Mechanical Engineering, Power Generation, Components for high heat resistant pipelines, steam boiler and turbine construction and parts for the chemical industry and reactor technology

Processing history

Quenched and Tempered