Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 20-250 mm

Mechanical

PropertyValue

Tensile strength

620.0 - 850.0 MPa

Show Supplier Material materials with Tensile strength of 620.0 - 850.0 MPa

Chemical properties

PropertyValueComment

Carbon

0.1 %

Show Supplier Material materials with Carbon of 0.1 %

max.

Chromium

17.0 - 19.0 %

Show Supplier Material materials with Chromium of 17.0 - 19.0 %

Manganese

2.0 %

Show Supplier Material materials with Manganese of 2.0 %

max.

Nickel

9.0 - 12.0 %

Show Supplier Material materials with Nickel of 9.0 - 12.0 %

Phosphorus

0.045 %

Show Supplier Material materials with Phosphorus of 0.045 %

max.

Sulfur

1.0 %

Show Supplier Material materials with Sulfur of 1.0 %

max.

Titanium

0.5 - 0.8 %

Show Supplier Material materials with Titanium of 0.5 - 0.8 %

Technological properties

Property
Application areas

Power plant engineering, Mechanical engineering, Power Generation, Fittings and accessories in boiler construction, Pipelines

Processing history

Quenched and Tempered