KetaSpire® PEEK MS NT1 AM Filament

Want to keep this datasheet? Save it now in your required format

Description

Ketaspire® MS NT1 AM Filament provides long-term performance up to 240°C, including exceptional chemical resistance, outstanding wear and abrasion resistance. These properties make it particularly suited for metal replacement in critical applications in severe end-use environments, such as Oil & Gas, Aerospace and Automotive.

This material data has been provided by Solvay Specialty Polymers.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

1.29 g/cm³

Show Supplier Material materials with Density of 1.29 g/cm³

ASTM D792

Dimension

PropertyValue

Diameter

1.75 mm

Show Supplier Material materials with Diameter of 1.75 mm

Mechanical

PropertyValueComment

Elastic modulus

3.12 GPa

Show Supplier Material materials with Elastic modulus of 3.12 GPa

ASTM D638

Elongation

26.0 %

Show Supplier Material materials with Elongation of 26.0 %

ASTM D638

Elongation at yield

4.8 %

Show Supplier Material materials with Elongation at yield of 4.8 %

ASTM D638

Impact strength, Izod notched, ASTM

81.0 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 81.0 J/m

ASTM D256

Tensile strength

48.0 MPa

Show Supplier Material materials with Tensile strength of 48.0 MPa

ASTM D638

Yield strength

85.0 MPa

Show Supplier Material materials with Yield strength of 85.0 MPa

ASTM D638

Thermal

PropertyValueComment

Melting point

343.0 °C

Show Supplier Material materials with Melting point of 343.0 °C

ASTM D3418

Technological properties

Property
Application areas

Aerospace Applications, Automotive Applications, Oil/Gas Applications

Certifications

Substances used to manufacture the polymer grade used for this filament meets the requirements of Commission Regulation (EU) N°10/2011, which implements the framework regulation EU 1935/2004 as related to plastic materials and articles intended to come into contact with food and its subsequent amendments as well as the GMP requirements for EU 2023/2006.


Please feel free to contact the supplier for RoHS Compliance.

Color

Natural

Features

  • Chemical Resistant
  • Ductile
  • Flame Retardant
  • Good Dimensional Stability
  • Good Impact Resistance
  • High Heat Resistance
  • Other

    Test specimen parameters:

  • First layer: 0.3mm thick
  • Subsequent layers: 0.1mm
  • 100% infill
  • 3 shells
  • Printing speed: 18 mm/s

  • Note:

    Typical properties: these are not to be construed as specifications

    Processing methods

    Fused Filament Fabrication (FFF)


    Printing conditions for above data table:

  • Filament drying conditions, minimum temperature 4h: 150°C
  • Extruder temperature: 400-440°C
  • Bed temperature: 180-220°C
  • Printing tool path: cross hatching in the XY plane
  • Do you have a technical question or need more information about this material?

    Post it as a comment below and receive answers from engineers and other community members.