Description

Solef® PVDF AM Filament MSC NT 1 provides long term performance up to 120°C, including exceptional chemical resistance and outstanding UV, weathering and oxidation resistance. The product is also intrinsically endowed of a very high purity. These features make it particularly suited for outdoor applications, and applications in contact with harsh chamical environments, such as Chemical Processing Industry, Semiconductor Industry and Oil&Gas.

This material data has been provided by Solvay Specialty Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.72 g/cm³

Show Supplier Material materials with Density of 1.72 g/cm³

ASTM D792, ¹

Dimension

PropertyValue

Diameter

2.85 mm

Show Supplier Material materials with Diameter of 2.85 mm

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

0.8 GPa

Show Supplier Material materials with Elastic modulus of 0.8 GPa

ASTM D638, ²

Elongation

23.0 °C

50 - 250 %

Show Supplier Material materials with Elongation of 50 - 250 %

ASTM D638, ²

Elongation at yield

23.0 °C

10 %

Show Supplier Material materials with Elongation at yield of 10 %

ASTM D638, ²

Impact strength, Charpy notched

23.0 °C

6 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m²

Tensile strength

23.0 °C

25 MPa

Show Supplier Material materials with Tensile strength of 25 MPa

ASTM D638

Yield strength

23.0 °C

30 MPa

Show Supplier Material materials with Yield strength of 30 MPa

ASTM D638, ²

Thermal

PropertyValueComment

Melting point

148 °C

Show Supplier Material materials with Melting point of 148 °C

ASTM D3418

Technological properties

Property
Application areas

Additive Manufacturing (3D Printing), Industrial applications, Oil/Gas applications, Plumbing applications

Certifications

Substances used to manufacture the polymer grade used for this filament meets the requirements of Commission Regulation (EU) N°10/2011, which implements the framework regulation EU 1935/2004 as related to plastic materials and articles intended to come into contact with food and its subsequent amendments as well as the GMP requirements for EU 2023/2006.


Please feel free to contact the supplier for RoHS Compliance.

Color

White

Features

  • Chemical Resistant
  • Flame Retardant
  • Good weather resistance
  • High Purity
  • Oxidation Resistant
  • UV Resistant
  • Other

    Test specimen parameters:

  • Layer thickness: 0.2mm thick
  • 100% infill
  • 3 shells
  • Printing speed: 25 mm/s

  • Note:

    Typical properties: these are not to be construed as specifications

    ¹On 3D printed specimens

    ²On 3D printed specimens, x-direction

    Processing methods

    Fused Filament Fabrication (FFF)


    Printing conditions for above data table:

  • Filament drying conditions: drying not needed
  • Extruder temperature: 225-235°C
  • Bed temperature: 100°C
  • Printing tool path: cross hatching in the XY plane