AISI 4130 Annealed

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by Songshun Steel.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.8 g/cm³

Show Supplier Material materials with Density of 7.8 g/cm³

Dimension

PropertyValueComment

Length

1000 - 6000 mm

Show Supplier Material materials with Length of 1000 - 6000 mm

Thickness

800 mm

Show Supplier Material materials with Thickness of 800 mm

max.

Width

205 - 2300 mm

Show Supplier Material materials with Width of 205 - 2300 mm

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

200 - 210 GPa

Show Supplier Material materials with Elastic modulus of 200 - 210 GPa

Typical for Steels

Elongation

23.0 °C

28.2 %

Show Supplier Material materials with Elongation of 28.2 %

Hardness, Brinell

23.0 °C

156 [-]

Show Supplier Material materials with Hardness, Brinell of 156 [-]

Poisson's ratio

23.0 °C

0.29 [-]

Show Supplier Material materials with Poisson's ratio of 0.29 [-]

Typical for Steels

Reduction of area

23.0 °C

55.6 %

Show Supplier Material materials with Reduction of area of 55.6 %

Tensile strength

23.0 °C

560 MPa

Show Supplier Material materials with Tensile strength of 560 MPa

Yield strength

23.0 °C

360 MPa

Show Supplier Material materials with Yield strength of 360 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.2E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.2E-5 1/K

Specific heat capacity

23.0 °C

477 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 477 J/(kg·K)

Thermal conductivity

23.0 °C

42.7 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 42.7 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

2.2E-7 Ω·m

Show Supplier Material materials with Electrical resistivity of 2.2E-7 Ω·m

Chemical properties

PropertyValue

Carbon

0.28 - 0.33 %

Show Supplier Material materials with Carbon of 0.28 - 0.33 %

Chromium

0.8 - 1.1 %

Show Supplier Material materials with Chromium of 0.8 - 1.1 %

Copper

0.35 %

Show Supplier Material materials with Copper of 0.35 %

Iron

Balance

Manganese

0.4 - 0.6 %

Show Supplier Material materials with Manganese of 0.4 - 0.6 %

Molybdenum

0.15 - 0.25 %

Show Supplier Material materials with Molybdenum of 0.15 - 0.25 %

Nickel

0.25 %

Show Supplier Material materials with Nickel of 0.25 %

Phosphorus

0.03 %

Show Supplier Material materials with Phosphorus of 0.03 %

Silicon

0.15 - 0.35 %

Show Supplier Material materials with Silicon of 0.15 - 0.35 %

Sulfur

0.04 %