PropertyTemperatureValueComment

Elastic modulus

23.0 °C

200 - 210 GPa

Show Supplier Material materials with Elastic modulus of 200 - 210 GPa

Typical for Steels

Hardness, Rockwell C

23.0 °C

47 - 49 [-]

Show Supplier Material materials with Hardness, Rockwell C of 47 - 49 [-]

Tempered

Hardness, Brinell

Annealed

Chemical properties

PropertyValue

Carbon

0.45 %

Show Supplier Material materials with Carbon of 0.45 %

Chromium

4.75 - 5.5 %

Show Supplier Material materials with Chromium of 4.75 - 5.5 %

Iron

Balance

Manganese

0.2 - 0.5 %

Show Supplier Material materials with Manganese of 0.2 - 0.5 %

Molybdenum

1.1 - 1.75 %

Show Supplier Material materials with Molybdenum of 1.1 - 1.75 %

Phosphorus

0.03 %

Show Supplier Material materials with Phosphorus of 0.03 %

Silicon

0.8 - 1.2 %

Show Supplier Material materials with Silicon of 0.8 - 1.2 %

Sulfur

0.03 %

Show Supplier Material materials with Sulfur of 0.03 %

Vanadium

0.9 - 1.1 %

Show Supplier Material materials with Vanadium of 0.9 - 1.1 %