1.2714

Want to keep this datasheet? Save it now in your required format

This material data has been provided by Songshun Steel.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValueComment

Diameter

20 - 800 mm

Show Supplier Material materials with Diameter of 20 - 800 mm

Length

3000 - 5800 mm

Show Supplier Material materials with Length of 3000 - 5800 mm

Thickness

800 mm

Show Supplier Material materials with Thickness of 800 mm

max.

Width

205 - 800 mm

Show Supplier Material materials with Width of 205 - 800 mm

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

200 - 210 GPa

Show Supplier Material materials with Elastic modulus of 200 - 210 GPa

Typical for Steels

Hardness, Brinell

23.0 °C

240 [-]

Show Supplier Material materials with Hardness, Brinell of 240 [-]

Annealed

Hardness, Rockwell C

23.0 °C

45 [-]

Show Supplier Material materials with Hardness, Rockwell C of 45 [-]

Hardened and Tempered

Chemical properties

PropertyValue

Carbon

0.5 - 0.6 %

Show Supplier Material materials with Carbon of 0.5 - 0.6 %

Chromium

1 - 1.2 %

Show Supplier Material materials with Chromium of 1 - 1.2 %

Iron

Balance

Manganese

0.65 - 0.95 %

Show Supplier Material materials with Manganese of 0.65 - 0.95 %

Molybdenum

0.45 - 0.55 %

Show Supplier Material materials with Molybdenum of 0.45 - 0.55 %

Nickel

1.5 - 1.8 %

Show Supplier Material materials with Nickel of 1.5 - 1.8 %

Phosphorus

0.03 %

Show Supplier Material materials with Phosphorus of 0.03 %

Silicon

0.1 - 0.4 %

Show Supplier Material materials with Silicon of 0.1 - 0.4 %

Sulfur

0.03 %

Show Supplier Material materials with Sulfur of 0.03 %

Vanadium

0.07 - 0.12 %

Show Supplier Material materials with Vanadium of 0.07 - 0.12 %