ABS HI121

Alternative and trade names
HI121
Want to keep this datasheet? Save it now in your required format

Description

Well Balanced Mechanical Properties

This material data has been provided by Toling Corporation Sdn Bhd .

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.04 g/cm³

Show Supplier Material materials with Density of 1.04 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.08 GPa

Show Supplier Material materials with Elastic modulus of 2.08 GPa

ASTM D638

Elongation

23.0 °C

40 %

Show Supplier Material materials with Elongation of 40 %

ASTM D638

Flexural modulus

23.0 °C

2.45 GPa

Show Supplier Material materials with Flexural modulus of 2.45 GPa

ASTM D790

Flexural strength

23.0 °C

72.6 MPa

Show Supplier Material materials with Flexural strength of 72.6 MPa

ASTM D790

Hardness, Rockwell R

23.0 °C

108 [-]

Show Supplier Material materials with Hardness, Rockwell R of 108 [-]

ASTM D785

Yield strength

23.0 °C

45.1 MPa

Show Supplier Material materials with Yield strength of 45.1 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

91 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 91 °C

ASTM D648

Heat deflection temperature, 1.80 MPa

87 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 87 °C

ASTM D648

Relative temperature index, electrical

60 °C

Show Supplier Material materials with Relative temperature index, electrical of 60 °C

UL 746B

Relative temperature index, mechanical impact

60 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 60 °C

UL 746B

Relative temperature index, mechanical strength

60 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 60 °C

UL 746B

Vicat softening temperature

93 °C

Show Supplier Material materials with Vicat softening temperature of 93 °C

ASTM D1525

Flammability

HB UL94

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

0 V

Show Supplier Material materials with Comparative tracking index of 0 V

IEC 60112

Rheological Properties

PropertyValueComment

Melt mass-flow rate

21 g/10min

Show Supplier Material materials with Melt mass-flow rate of 21 g/10min

ASTM D1238

Technological properties

Property
Application areas

ELECTRIC & ELECTRONIC, MISCELLANEOUS GOODS