Property | Value | Temperature | Comment |
---|---|---|---|
Lateral flake size | 10000 nm Show Supplier Material materials with Lateral flake size of 10000 nm | Using SEM | |
Layer number | 1 - 10 [-] Show Supplier Material materials with Layer number of 1 - 10 [-] | ≤5 is 60%, ≤10 is 90% and >10 is 10%, using Raman | |
Layer thickness | 3.5 µm Show Supplier Material materials with Layer thickness of 3.5 µm at 23.0 °C | 23.0 °C |
Mechanical
Thermal
Property | Value | Temperature |
---|---|---|
Thermal conductivity | 5000 W/(m·K) Show Supplier Material materials with Thermal conductivity of 5000 W/(m·K) at 23.0 °C | 23.0 °C |
Chemical properties
Property | ||
---|---|---|
Carbon | 97 - 99 % | |
Fluorine | 0 - 1 % | |
Nitrogen | 0 - 0.6 % | |
Oxygen | 1 - 3 % | |
Sulfur | 0 - 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Being electrically conductive, thermally conductive and a highly effective mechanical reinforcer there are numerous potential applications for graphene such as: composites, energy, biomedical, membranes, coatings, sensors, electronics |