Description

GNP-HP is a few-layer graphene powder with large lateral dimensions. With a defect ratio to match Nanene™, GNP-HP is suitable for a wide range of applications and has shown significant improvements in tensile strength, Young’s modulus, uniform elongation and elongation at break.

This material data has been provided by Versarien.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Lateral flake size

26500 nm

Show Supplier Material materials with Lateral flake size of 26500 nm

Using SEM

Layer number

1 - 100 [-]

Show Supplier Material materials with Layer number of 1 - 100 [-]

≤5 is 18%, ≤10 is 73% and 10-100 is 27%, using Raman

Chemical properties

Property

Carbon

93 - 99 %

Fluorine

0 - 2 %

Nitrogen

0 - 0.6 %

Oxygen

1 - 5 %

Sulfur

0 - 2 %

Technological properties

Property
Application areas

Being electrically conductive, thermally conductive and a highly effective mechanical reinforcer there are numerous potential applications for graphene such as: composites, energy, biomedical, membranes, coatings, sensors, electronics