GRAPHINK 2

Alternative and trade names
GRAPHINK 2
Want to keep this datasheet? Save it now in your required format

Description

Our own graphene inks are produced via a patented micro-fluidisation process. Printable conductive inks for flexible electronics can be both cheaper and more flexible than traditional circuit board solutions. We have two different inks suitable for different deposition methods. Both are environmentally friendly, non-toxic, aqueous and can be stored at room temperature (20°C). We also formulate graphene inks for specific customer requirements. Solvent: Water, Solid content: 10.3 wt%, Graphene content: 100 mg/mL, Transparent films can not be coated, Transparent substrates: Glass, Paper and Plastics

This material data has been provided by Versarien.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Lateral flake size

500.0 - 1500.0 nm

Show Supplier Material materials with Lateral flake size of 500.0 - 1500.0 nm

Layer thickness

0.005 - 0.015 µm

Show Supplier Material materials with Layer thickness of 0.005 - 0.015 µm

Electrical

PropertyValueComment

Surface resistivity

10.0 Ω/sq

Show Supplier Material materials with Surface resistivity of 10.0 Ω/sq

For 25µm thickness

Rheological Properties

PropertyValue

Viscosity

0.6000000000000001 Pa·s

Show Supplier Material materials with Viscosity of 0.6000000000000001 Pa·s

Technological properties

Property
Application areas

flexible electronics

Processing methods

Flexo, Gravure, Screen Printing, Blade, Meyer Bar Coating - with a drying condition of 100℃ for 10 min