GO Graphene Powder

Alternative and trade names
GO
Want to keep this datasheet? Save it now in your required format

Description

In addition to our high quality, low defect graphene powders, we also supply graphene oxide. With a higher defect ratio, these products are suitable for different applications where the high proportion of oxygen would be beneficial.

This material data has been provided by Versarien.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Lateral flake size

4000 nm

Show Supplier Material materials with Lateral flake size of 4000 nm

Using SEM/AFM

Layer number

1 - 2 [-]

Show Supplier Material materials with Layer number of 1 - 2 [-]

Using AFM

Chemical properties

PropertyValue

Carbon

55 - 65 %

Show Supplier Material materials with Carbon of 55 - 65 %

Manganese

0 - 3 %

Show Supplier Material materials with Manganese of 0 - 3 %

Nitrogen

0 - 3 %

Show Supplier Material materials with Nitrogen of 0 - 3 %

Oxygen

28 - 38 %

Show Supplier Material materials with Oxygen of 28 - 38 %

Sulfur

0 - 5 %

Show Supplier Material materials with Sulfur of 0 - 5 %

Technological properties

Property
Application areas

li-ion batteries, fuel cells , battery electrodes, solar pv cells, electrically conductive inks, thermally conductive films and coatings, thermal interface materials, lightweight composites, concrete, metal -matrix composites, corrosion protection, barrier properties / permeation / mechanical performance

Color

Brown