General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 12.7 g/cm³ Show Material materials with Density of 12.7 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Flexural strength | 20.0 °C | 758 - 827 MPa Show Material materials with Flexural strength of 758 - 827 MPa |
Hardness, Rockwell B | 20.0 °C | 77 - 90 [-] Show Material materials with Hardness, Rockwell B of 77 - 90 [-] |
Tensile strength | 20.0 °C | 379 - 448 MPa Show Material materials with Tensile strength of 379 - 448 MPa |
Electrical
Property | Value |
---|---|
Specific Electrical conductivity | 34 - 57 % IACS Show Material materials with Specific Electrical conductivity of 34 - 57 % IACS |
Chemical properties
Property | Value |
---|---|
Copper | 38 - 42 % Show Material materials with Copper of 38 - 42 % |