General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 19.3 g/cm³ Show Material materials with Density of 19.3 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 20.0 °C | 405 - 407 GPa Show Material materials with Elastic modulus of 405 - 407 GPa |
Hardness, Vickers | 20.0 °C | 360 [-] Show Material materials with Hardness, Vickers of 360 [-] |
Poisson's ratio | 20.0 °C | 0.28 [-] Show Material materials with Poisson's ratio of 0.28 [-] |
Shear modulus | 20.0 °C | 166 GPa Show Material materials with Shear modulus of 166 GPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 4.5E-6 - 4.6E-6 1/K Show Material materials with Coefficient of thermal expansion of 4.5E-6 - 4.6E-6 1/K | Typical for Tungsten |
Melting point | 3410 °C Show Material materials with Melting point of 3410 °C | Typical for Tungsten | |
Specific heat capacity | 23.0 °C | 134 - 142 J/(kg·K) Show Material materials with Specific heat capacity of 134 - 142 J/(kg·K) | Typical for Tungsten |
Thermal conductivity | 20.0 °C | 4.2 - 167 W/(m·K) Show Material materials with Thermal conductivity of 4.2 - 167 W/(m·K) | |
1000.0 °C | 111 W/(m·K) Show Material materials with Thermal conductivity of 111 W/(m·K) | ||
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 20.0 °C | 5.5E-8 Ω·m Show Material materials with Electrical resistivity of 5.5E-8 Ω·m |
1000.0 °C | 3.26E-7 Ω·m Show Material materials with Electrical resistivity of 3.26E-7 Ω·m | |
1500.0 °C | 4.86E-7 Ω·m Show Material materials with Electrical resistivity of 4.86E-7 Ω·m | |
2000.0 °C | 6.71E-7 Ω·m Show Material materials with Electrical resistivity of 6.71E-7 Ω·m | |
Chemical properties
Property | Value |
---|---|
Carbon | 0.01 % Show Material materials with Carbon of 0.01 % |
Iron | 0.01 % Show Material materials with Iron of 0.01 % |
Nickel | 0.01 % Show Material materials with Nickel of 0.01 % |
Nitrogen | 0.01 % Show Material materials with Nitrogen of 0.01 % |
Oxygen | 0.01 % Show Material materials with Oxygen of 0.01 % |
Silicon | 0.01 % Show Material materials with Silicon of 0.01 % |
Tungsten | 99.95 % Show Material materials with Tungsten of 99.95 % |