General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 17.75 - 18.35 g/cm³ Show Material materials with Density of 17.75 - 18.35 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 20.0 °C | 360 - 380 GPa Show Material materials with Elastic modulus of 360 - 380 GPa |
Elongation | 20.0 °C | 1 - 3 % Show Material materials with Elongation of 1 - 3 % |
Hardness, Rockwell C | 20.0 °C | 34 [-] Show Material materials with Hardness, Rockwell C of 34 [-] |
Shear modulus | 20.0 °C | 140 - 150 GPa Show Material materials with Shear modulus of 140 - 150 GPa |
Tensile strength | 20.0 °C | 648 - 724 MPa Show Material materials with Tensile strength of 648 - 724 MPa |
Yield strength Rp0.2 | 20.0 °C | 517 MPa Show Material materials with Yield strength Rp0.2 of 517 MPa |
Chemical properties
Property | Value |
---|---|
Tungsten | 95 % Show Material materials with Tungsten of 95 % |