General
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Density | 20.0 °C | 2.65 g/cm³ Show Material materials with Density of 2.65 g/cm³ | T5 | DIN 1725-2, EN 1676, EN 1706 |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Elastic modulus | 20.0 °C | 74.0 GPa Show Material materials with Elastic modulus of 74.0 GPa | T5 | DIN 1725-2, EN 1676, EN 1706 | |
Elongation | 20.0 °C | 2.0 % Show Material materials with Elongation of 2.0 % | T5 | DIN 1725-2, EN 1676, EN 1706 | |
20.0 °C | 2.0 - 5.0 % Show Material materials with Elongation of 2.0 - 5.0 % | T5 | DIN 1725-2, EN 1676, EN 1706 | ||
20.0 °C | 3.0 % Show Material materials with Elongation of 3.0 % | T5 | DIN 1725-2, EN 1676, EN 1706 | ||
20.0 °C | 4.0 - 7.0 % Show Material materials with Elongation of 4.0 - 7.0 % | T5 | DIN 1725-2, EN 1676, EN 1706 | ||
Hardness, Brinell | 20.0 °C | 75.0 [-] Show Material materials with Hardness, Brinell of 75.0 [-] | T5 | DIN 1725-2, EN 1676, EN 1706 | |
20.0 °C | 75.0 - 110.0 [-] Show Material materials with Hardness, Brinell of 75.0 - 110.0 [-] | T5 | DIN 1725-2, EN 1676, EN 1706 | ||
20.0 °C | 80.0 [-] Show Material materials with Hardness, Brinell of 80.0 [-] | T5 | DIN 1725-2, EN 1676, EN 1706 | ||
20.0 °C | 80.0 - 115.0 [-] Show Material materials with Hardness, Brinell of 80.0 - 115.0 [-] | T5 | DIN 1725-2, EN 1676, EN 1706 | ||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | |||
Shear modulus | 2.8 GPa Show Material materials with Shear modulus of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | |||
Tensile strength | 20.0 °C | 220.0 MPa Show Material materials with Tensile strength of 220.0 MPa | T5 | DIN 1725-2, EN 1676, EN 1706 | |
20.0 °C | 230.0 - 300.0 MPa Show Material materials with Tensile strength of 230.0 - 300.0 MPa | T5 | DIN 1725-2, EN 1676, EN 1706 | ||
20.0 °C | 240.0 MPa Show Material materials with Tensile strength of 240.0 MPa | T5 | DIN 1725-2, EN 1676, EN 1706 | ||
20.0 °C | 250.0 - 340.0 MPa Show Material materials with Tensile strength of 250.0 - 340.0 MPa | T5 | DIN 1725-2, EN 1676, EN 1706 |
Thermal
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 200.0 °C | 2.2e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.2e-05 1/K | T5 | DIN 1725-2, EN 1676, EN 1706 | |
Melting point | 505.0 - 770.0 °C Show Material materials with Melting point of 505.0 - 770.0 °C | Typical for Cast 3xx.x Series Aluminium | |||
Specific heat capacity | 20.0 °C | 910.0 J/(kg·K) Show Material materials with Specific heat capacity of 910.0 J/(kg·K) | T5 | DIN 1725-2, EN 1676, EN 1706 | |
Thermal conductivity | 20.0 °C | 140.0 - 170.0 W/(m·K) Show Material materials with Thermal conductivity of 140.0 - 170.0 W/(m·K) | T5 | DIN 1725-2, EN 1676, EN 1706 |
Electrical
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Electrical conductivity | 20.0 °C | 20000000.0 - 23000000.0 S/m Show Material materials with Electrical conductivity of 20000000.0 - 23000000.0 S/m | T5 | DIN 1725-2, EN 1676, EN 1706 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminium | 88.9 % Show Material materials with Aluminium of 88.9 % | T5 | DIN 1725-2, EN 1676, EN 1706 |
Copper | 0.05 Show Material materials with Copper of 0.05 | T5 | DIN 1725-2, EN 1676, EN 1706 |
Iron | 0.18 Show Material materials with Iron of 0.18 | T5 | DIN 1725-2, EN 1676, EN 1706 |
Magnesium | 0.25 - 0.45 % Show Material materials with Magnesium of 0.25 - 0.45 % | T5 | DIN 1725-2, EN 1676, EN 1706 |
Manganese | 0.1 Show Material materials with Manganese of 0.1 | T5 | DIN 1725-2, EN 1676, EN 1706 |
Silicon | 9.0 - 10.0 % Show Material materials with Silicon of 9.0 - 10.0 % | T5 | DIN 1725-2, EN 1676, EN 1706 |
Titanium | 0.15 Show Material materials with Titanium of 0.15 | T5 | DIN 1725-2, EN 1676, EN 1706 |
Zinc | 0.07 Show Material materials with Zinc of 0.07 | T5 | DIN 1725-2, EN 1676, EN 1706 |
Technological properties
Property | ||
---|---|---|
Processing methods | permanent mould casting, sample taken from casting |